ZEIT Group
Contact Now

AL2O3 Atomic Layer Deposition Equipment For Nanostructure Pattern Industry

Brand Name : ZEIT

Model Number : ALD-NP-X—X

Certification : Case by case

Place of Origin : Chengdu, P.R.CHINA

MOQ : 1set

Price : Case by case

Payment Terms : T/T

Supply Ability : Case by case

Delivery Time : Case by case

Packaging Details : Wooden case

Weight : Customizable

Size : Customizable

Guarantee period : 1 year or case by case

Customizable : Available

Shipping Terms : By Sea / Air / Multimodal Transport

Contact Now

Atomic Layer Deposition in Nanostructure and Pattern Industry


Applications

Applications Specific Purpose
Nanostructure and pattern

Template-assisted nanostructure

Catalyst-assisted nanostructure
Regioselective ALD for nanopattern preparation


Working Principle
Atomic layer deposition is a method of forming film by making the gaseous phase precursors pulsed alternately
into the reaction chamber and producing the gas-solid phase chemisorption reaction on the deposited substrate
surface. When the precursors reach the surface of the deposited substrate, they will be chemically adsorbed on
the surface and produce the surface reactions.


Features

Model ALD-NP-X—X
Coating film system AL2O3, TiO2, ZnO, etc
Coating temperature range Normal temperature to 500℃ (Customizable)
Coating vacuum chamber size

Inner diameter: 1200mm, Height: 500mm (Customizable)

Vacuum chamber structure According to customer’s requirements
Background vacuum <5×10-7mbar
Coating thickness ≥0.15nm
Thickness control precision ±0.1nm
Coating size 200×200mm² / 400×400mm² / 1200×1200 mm², etc
Film thickness uniformity ≤±0.5%
Precursor and carrier gas

Trimethylaluminum, titanium tetrachloride, diethyl zinc, pure water,
nitrogen, etc.

Note: Customized production available.


Coating Samples

AL2O3 Atomic Layer Deposition Equipment For Nanostructure Pattern IndustryAL2O3 Atomic Layer Deposition Equipment For Nanostructure Pattern Industry

Process Steps
→ Place the substrate for coating into the vacuum chamber;
→ Vacuumize the vacuum chamber at high and low temperature, and rotate the substrate synchronously;
→ Start coating: the substrate is contacted with precursor in sequence and without simultaneous reaction;
→ Purge it with high-purity nitrogen gas after each reaction;
→ Stop rotating the substrate after the film thickness is up to standard and the operation of purging and cooling is

completed, then take out the substrate after the vacuum breaking conditions are met.

Our Advantages
We are manufacturer.
Mature process.
Reply within 24 working hours.


Our ISO Certification
AL2O3 Atomic Layer Deposition Equipment For Nanostructure Pattern Industry

Parts Of Our Patents
AL2O3 Atomic Layer Deposition Equipment For Nanostructure Pattern IndustryAL2O3 Atomic Layer Deposition Equipment For Nanostructure Pattern Industry

Parts Of Our Awards and Qualifications of R&D

AL2O3 Atomic Layer Deposition Equipment For Nanostructure Pattern IndustryAL2O3 Atomic Layer Deposition Equipment For Nanostructure Pattern Industry










Product Tags:

Nanostructure Atomic Layer Deposition

      

Pattern Industry Atomic Layer Deposition

      

AL2O3 Atomic Layer Deposition Equipment

      
Buy cheap AL2O3 Atomic Layer Deposition Equipment For Nanostructure Pattern Industry product

AL2O3 Atomic Layer Deposition Equipment For Nanostructure Pattern Industry Images

Inquiry Cart 0
Send your message to this supplier
 
*From:
*To: ZEIT Group
*Subject:
*Message:
Characters Remaining: (0/3000)