Separation Membrane Field Filtration Atomic Layer Deposition ALD Machine

Brand Name : ZEIT

Model Number : ALD-SM-X—X

Certification : Case by case

Place of Origin : Chengdu, P.R.CHINA

MOQ : 1set

Price : Case by case

Payment Terms : T/T

Supply Ability : Case by case

Delivery Time : Case by case

Packaging Details : Wooden case

Weight : Customizable

Size : Customizable

Guarantee period : 1 year or case by case

Customizable : Available

Shipping Terms : By Sea / Air / Multimodal Transport

Contact Now

Atomic Layer Deposition in Separation Membrane field

Applications

Applications Specific Purpose
Separation membrane

Filtration

Gas separation

Working Principle
Atomic layer deposition (ALD) has the following advantages due to the surface saturation chemisorption and

self-limiting reaction mechanism:
1. Accurately control the film thickness by controlling the cycle numbers;
2. Due to the mechanism of surface saturation, there is no need to control the uniformity of precursor flow;
3. High uniform films can be generated;
4. Excellent step coverage with high aspect ratio.

Features

Model ALD-SM-X—X
Coating film system AL2O3, TiO2, ZnO, etc
Coating temperature range Normal temperature to 500℃ (Customizable)
Coating vacuum chamber size

Inner diameter: 1200mm, Height: 500mm (Customizable)

Vacuum chamber structure According to customer’s requirements
Background vacuum <5×10-7mbar
Coating thickness ≥0.15nm
Thickness control precision ±0.1nm
Coating size 200×200mm² / 400×400mm² / 1200×1200 mm², etc
Film thickness uniformity ≤±0.5%
Precursor and carrier gas

Trimethylaluminum, titanium tetrachloride, diethyl zinc, pure water,

nitrogen, etc.

Note: Customized production available.

Coating Samples

Separation Membrane Field Filtration Atomic Layer Deposition ALD MachineSeparation Membrane Field Filtration Atomic Layer Deposition ALD Machine

Process Steps
→ Place the substrate for coating into the vacuum chamber;
→ Vacuumize the vacuum chamber at high and low temperature, and rotate the substrate synchronously;
→ Start coating: the substrate is contacted with precursor in sequence and without simultaneous reaction;
→ Purge it with high-purity nitrogen gas after each reaction;
→ Stop rotating the substrate after the film thickness is up to standard and the operation of purging and cooling is

completed, then take out the substrate after the vacuum breaking conditions are met.

Our Advantages

We are manufacturer.

Mature process.

Reply within 24 working hours.

Our ISO Certification

Separation Membrane Field Filtration Atomic Layer Deposition ALD Machine

Parts Of Our Patents

Separation Membrane Field Filtration Atomic Layer Deposition ALD MachineSeparation Membrane Field Filtration Atomic Layer Deposition ALD Machine

Parts Of Our Awards and Qualifications of R&D

Separation Membrane Field Filtration Atomic Layer Deposition ALD MachineSeparation Membrane Field Filtration Atomic Layer Deposition ALD Machine


Product Tags:

Separation Membrane field Atomic Layer Deposition

      

Separation Membrane field ald machine

      

Filtration ald machine

      
Buy cheap Separation Membrane Field Filtration Atomic Layer Deposition ALD Machine product

Separation Membrane Field Filtration Atomic Layer Deposition ALD Machine Images

Inquiry Cart 0
Send your message to this supplier
 
*From:
*To: ZEIT Group
*Subject:
*Message:
Characters Remaining: (0/3000)